The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 28, 1998

Filed:

Sep. 03, 1996
Applicant:
Inventors:

Takeyoshi Doko, Tochigi, JP;

Koji Okada, Tochigi, JP;

Tokinori Onda, Tochigi, JP;

Hiroaki Takeuchi, Tochigi, JP;

Yoji Hirano, Tochigi, JP;

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B / ; F28F / ; F28F / ;
U.S. Cl.
CPC ...
428654 ; 428933 ; 1651341 ; 165905 ;
Abstract

A typical aluminum alloy brazing material includesover 7.0 wt. % and not more than 12.0 wt. % of Si: over 0.1 wt. % and not more than 8.0 wt. % of Cu. over 0.05 wt. % and not more than 0.5 wt. % or Fe, further at least one kind selected from a group consisting of over 0.5 wt. % and not more than 5.5 wt. % of Zn. over 0.002 wt. % and not more than 0.3 wt % of In and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al an inevitable impurities. A typical cladded aluminum alloy brazing sheet with a three-layer structure includes a brazing material, a core material comprising over 0.6 wt. % and not more than 2.5 wt. % of Si, over 0.5 wt. % and not more 2.5 wt. % of Cu, over 0.05 wt. % and not more than 2.0 wt. % of Mn, and the balance of Al and inevitable impurities, and a sacrificial material comprising at least one kind selected from a group consisting of over 0.5 wt. % and not more than 6.0 wt. % of Zn. over 0.002 wt. % and not more than 0.3 wt. % of In, and over 0.002 wt. % and not more than 0.3 wt. % of Sn, and the balance of Al and inevitable impurities, or comprises a core material cladded both sides thereof with the brazing material. By using the inventive brazing materials or brazing sheets, the brazing heating can be performed at a temperature of 570.degree. to 585.degree. C.