The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Sep. 30, 1997
Filed:
Dec. 09, 1994
V Durga Rao, Bloomfield Township, MI (US);
Robert Alan Rose, Grosse Pointe Park, MI (US);
David Alan Yeager, Plymouth, MI (US);
Daniel Michael Kabat, Oxford, MI (US);
Ford Global Technologies, Inc., Dearborn, MI (US);
Abstract
A method of making coated engine blocks by (a) casting a metallic engine block having one or more cylinder bores; (b) fabricating a thin walled liner for each bore, the liner being constituted of extruded metallic tubing having a cleansed inner surface, a wall thickness controlled to a thickness of 1-3 mm.+-.15 microns, the outer diameter of the liner being slightly greater than the internal diameter of the cylinder bores; (c) relatively rotating the liner with respect to one or more nozzles for applying a plurality of materials to the internal surface of the liner, the materials comprising first a metal texturing fluid that is applied at high pressures to expose fresh metal of the surface, secondly a bond coating material that is thermally sprayed to form a metallurgical bond with the liner internal surface, and a top coating of anti-friction material that is adheringly plasma sprayed to the bond coating; (d) honing the coated internal surface to remove up to 150 microns of top coating, leaving a finish surface that is concentric to the tube axis within .+-.15 microns; and (e) interference fitting the coated liner to the cylinder bore by freezing the liner while maintaining the block at or above ambient temperature to permit implanting of the liner.