The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Aug. 20, 1996
Filed:
Sep. 21, 1995
Yoshitaka Ito, Aichi, JP;
Masami Ishii, Aichi, JP;
Takayuki Nishio, Aichi, JP;
Uichiro Mizutani, Aichi, JP;
Yuh Yamada, Aichi, JP;
Fumihiko Ogasawara, Aichi, JP;
Motohiro Suganuma, Aichi, JP;
Aisin Seiki Kabushiki Kaisha, Kariya, JP;
Abstract
A superconductive ceramic composite material with high strength and capable of plastic deformation is prepared by mixing and sintering a superconductive powder represented by (RE.sub.x AE.sub.1-x).sub.1-y Cu.sub.y O.sub.z (RE represents Y or a rare-earth element having an atomic number of 57-71, or a combination of at least two of these elements, AE is at least one of alkaline earth elements Ca, Sr and Ba, x is 0.13-0.67, y is 0.25-0.67, and z is 1.08-1.17) and a metal powder M (M represents at least one of noble metals Rh, Pd, Ag, Ir, Pt and Au), in a defined ratio. The deformation (e.g., rolling) is followed by reheat-treatment (resintering). The powder mixture can be enclosed in a metallic capsule or made into a clad sheet by interposing the powder within two metallic sheets, and deformed (drawn or press formed into a desired shape) followed by sintering. The composite material may contain a superconductive network of such grains.