The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 28, 1996

Filed:

Mar. 30, 1995
Applicant:
Inventors:

David P Burgess, Mentor, OH (US);

Wendy M Gort, Winkelman, AZ (US);

Ronald K Haines, Mentor, OH (US);

Jackson G Jenkins, Oracle, AZ (US);

Stephen J Kohut, Chandler, AZ (US);

Peter Peckham, Concord, OH (US);

Assignee:

ElectroCopper Products Limited, Chandler, AZ (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C25C / ;
U.S. Cl.
CPC ...
205 74 ; 205574 ; 205575 ; 205580 ; 205583 ; 205585 ;
Abstract

This invention is directed to a process for making copper metal powder from copper-bearing material, comprising: (A) contacting said copper-beating material with an effective amount of at least one aqueous leaching solution to dissolve copper ions in said leaching solution and form a copper-rich aqueous leaching solution; (B) contacting said copper-rich aqueous leaching solution with an effective amount of at least one water-insoluble extractant to transfer copper ions from said copper-rich aqueous leaching solution to said extractant to form a copper-rich extractant and a copper-depleted aqueous leaching solution, said extractant comprising (i) at least one oxime characterized by a hydrocarbon linkage with at least one --OH group and at least one .dbd.NOH group attached to different carbon atoms on said hydrocarbon linkage, (ii) at least one betadiketone, or (iii) at least one ion-exchange resin; (C) separating said copper-rich extractant from said copper-depleted aqueous leaching solution; (D) contacting said copper-rich extractant with an effective amount of at least one aqueous stripping solution to transfer copper ions from said extractant to said stripping solution to form a copper-rich stripping solution and a copper-depleted extractant; (E) separating said copper-rich stripping solution from said copper-depleted extractant to form a first electrolyte solution; (F) advancing said first electrolyte solution to an electrolytic cell equipped with at least one first anode and at least one first cathode, and applying an effective amount of voltage across said first anode and said first cathode to deposit copper metal powder on said first cathode; and (G) removing copper metal powder from said first cathode. In one embodiment the copper metal powder is converted to copper foil. In one embodiment the copper metal powder is converted to cuprous oxide, cupric oxide or a mixture thereof; these copper oxides can be readily dissolved in sulfuric acid and used to make copper foil.