The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 24, 1995

Filed:

Dec. 22, 1993
Applicant:
Inventors:

Toru Koyama, Hitachi, JP;

Koo Honjo, Ibaraki, JP;

Masao Suzuki, Hitachi, JP;

Akio Takahashi, Hitachiota, JP;

Akio Mukoh, Mito, JP;

Keiji Fukushi, Hitachi, JP;

Seiji Numata, Hitachi, JP;

Assignee:

Hitachi, Ltd., Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B / ;
U.S. Cl.
CPC ...
428457 ; 4284735 ; 4284744 ; 428458 ; 428930 ; 505884 ; 505887 ; 505813 ; 505705 ; 1741251 ; 335216 ;
Abstract

A superconducting magnet coil contains a coil of superconducting wire and a cured product of a curable resin composition with which the coil has been impregnated, the cured product having a thermal shrinkage factor of 1.5-0.3%, preferably 1.0-0.3%, when cooled from the glass transition temperature to 4.2K, a bend-breaking strain of 2.9-3.9%, preferably 3.2-3.9%, at 4.2K and a modulus of 500-1,000 kg/mm.sup.2 at 4.2K, or undergoing a thermal stress of 0-10 kg/mm.sup.2 when cooled from the glass transition temperature to 4.2K and resisting to quench during superconducting operation. It is produced by winding a superconducting wire to form a coil; impregnating the coil with a curable resin composition of low viscosity which contains for example at least one epoxy resin selected from the group consisting of diglycidyl ether of bisphenol A, diglycidyl ether of bisphenol F and diglycidyl ether of bisphenol AF, all having a number-average molecular weight of 350-1,000, a flexibilizer and a curing catalyst, to obtain a curable-resin composition-impregnated coil; and heating the curable-resin-composition-impregnated coil to cure the composition.