The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Sep. 14, 1993
Filed:
Jul. 31, 1992
Yoshihiro Oshibe, Aichi, JP;
Yasuhiro Yamamoto, Aichi, JP;
Hiroshi Ohmura, Aichi, JP;
Keiji Kumazawa, Aichi, JP;
Nippon Oil and Fats Co., Ltd., Tokyo, JP;
Abstract
An ultraviolet curing antifogging agent is disclosed. The composition includes block copolymer (a) having a hydrophilic polymer segment (a1) and a hydrophobic polymer segment (a2). A polar solvent (c) is provided in which the hydrophilic polymer segment (a1) can easily be dissolved while the hydrophobic polymer segment (a2) can not. It further includes a photopolymerizable compound (b), and a photopolymerization initiator (d). The block copolymer (a) contains at least one hydrophilic monomer selected from the group of: a (meth) acrylamide compound represented by the general formula: CH.sub.2 .dbd.CR.sub.1 CONR.sub.2 R.sub.3 ; a cyclic (meth)acrylamide compound represented by the general formula ##STR1## and a hydroxyalkyl (meth)acrylate. Further, the hydrophilic polymer segment (a1) is formed by a radically polymerizable monomer having a functional group such as glycidyl group. The hydrophobic polymer segment (a2) is formed by a radically polymerizable monomer and a hydrophobic monomer which is copolymerizable with the former radically polymerizable monomer. The weight ratio of the hydrophilic polymer segment (a1) to the hydrophobic polymer segment (a2) is 50/50 to 95/5. The photopolymerizable compound (b) can be represented by the general formula CH.sub.2 .dbd.CR.sub.1 COO(CH.sub.2 CR.sub.4 HO).sub.n OCCR.sub.1 .dbd.CH.sub.2. The weight ratio of the component (a) to the component (b) is in the range of 10/90 to 90/10 in terms of the solid content. Such compositions have excellent antifogging properties and can be applied to transparent plastic materials to prevent fogging.