The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 1992

Filed:

Jul. 26, 1990
Applicant:
Inventors:

Darrell L Gallup, Chino Hills, CA (US);

Allen W Doty, Pomona, CA (US);

Morton M Wong, Placentia, CA (US);

Charles F Wong, Yorba Linda, CA (US);

John L Featherstone, El Centro, CA (US);

Jessie P Reverente, El Centro, CA (US);

Philip H Messer, Palm Desert, CA (US);

Assignee:

Union Oil Company of California, Los Angeles, CA (US);

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22B / ; C22B / ; C01G / ; C01G / ;
U.S. Cl.
CPC ...
423 42 ; 75726 ; 75733 ; 75736 ; 75744 ; 266170 ; 423D / ;
Abstract

Geothermal brine is passed through a zone containing a packing metal so as to reduce its tendency to deposit iron/silica scale, reduce corrosivity of the brine, and/or remove and recover metals from the brine. The method polished the geothermal brine by contacting the brine with a packing metal higher in the electromotive series than silver for a time sufficient for a precious metals to precipitate onto the packing at brine temperature and pH conditions which inhibit iron-rich silica scale. Most preferably, the contacting is accomplished near an injection well at the end of a heat extraction process and the packing comprises coiled zinc-galvanized steel chicken wire mesh packed in a sufficient density to also act as a filter for suspended particles. Alternatively, contacting is also accomplished near the production well. Dissolving the packing in a suitable acid leaves a precious metal-rich residue behind for subsequent recovery. When the brine is treated in accordance with this method, the useful life of injection wells used to return cooled brine back to the geothermal field is extended by at least about 3 time as compared to that observed with untreated brine. Further the contacted brine is less corrosive than it was before contacting.