The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 11, 1989

Filed:

May. 11, 1987
Applicant:
Inventors:

Masatoshi Tsuchitani, Ichihara, JP;

Sakae Naito, Chiba, JP;

Ryoichi Nakajima, Ichihara, JP;

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C10C / ;
U.S. Cl.
CPC ...
208 40 ; 208 22 ; 208 39 ; 208 44 ; 4234471 ; 4234472 ; 4234474 ;
Abstract

A process for the preparation of an excellent mesophase pitch suitable for use as a spinning pitch for the production of high performance carbon fibers is disclosed. The mesophase pitch can satisfy the four remarkable characteristics at the same time, i.e., a softening point of below 320.degree. C. as determined by Mettler method, a mesophase content of above 90% as examined on a polarized microscope, a quinoline insoluble content of less than 20%, and a xylene soluble content of less than 20%. The mesophase pitch is particularly homogeneous and is easily spinnable. The process can be characterized by a preliminary extraction step, a continuous heat treatment step, and an extraction step. In some cases, the preliminary extraction step can be omitted. Graphite fibers having a tensile strength of about 400 Kg/mm.sup.2 and a modulus of elasticity of above 60 ton/mm.sup.2 can be obtained from the mesophase pitch. Further, even carbon fibers prepared at a carbonization temperature of 1000.degree. C. have a tensile strength of about 300 Kg/mm.sup.2.