The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 21, 1989

Filed:

Oct. 21, 1987
Applicant:
Inventors:

Rainer Konrad, Goennheim, DE;

Guido Funk, Worms, DE;

Juergen Schmidt-Thuemmes, Ludwigshafen, DE;

Rudolf Mueller-Mall, Neuhofen, DE;

Guenther Schweier, Friedelsheim, DE;

Assignee:

BASF Aktiengesellschaft, Ludwigshafen, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F / ;
U.S. Cl.
CPC ...
502107 ; 502114 ; 502117 ; 502162 ; 502210 ; 526105 ;
Abstract

Ethene polymerization by Phillips catalysis is carried out using (1) a supported catalyst, which is laden with chromium, phosphorus and aluminum, and (2) a cocatalyst, (1) being obtained by a method in which (1.1) a catalyst intermediate laden with chromium, phosphorus and aluminum is prepared from a silicate carrier, a selected chromium compound, a selected phosphorus compound and a selected aluminum compound, and then (1.2) the catalyst intermediate is heated in an oxygen-containing gas stream. In this process, the component (1) used is one which is obtained by a method in which, in each case in a specific manner, (1.1) in a first stage, (1.1.1) first a suspension is prepared from (1.1.1.1) a finely divided silicate carrier and (1.1.1.2) an inert organic solvent, (1.1.2) then, (1.1.2.1) in an inert organic solvent, (1.1.2.2) an organic chromium compound is combined with (1.1.2.3) an aluminum trialkyl, (1.1.3) then (1.1.3.1) the suspension resulting from (1.1.1) is combined with (1.1.3.2) a phosphoric acid or phosphite and (1.1.3.3) the product obtained from (1.1.2), (1.1.4) finally, the suspension obtained in (1.1.3) is evaporated to dryness, and then (1.2) in a second stage, first (1.2.1) the intermediate obtained from (1.1) is treated with a stream of nitrogen, then (1.2.2) the intermediate obtained from (1.2.1) is heated in an oxygen-containing gas stream, and finally (1.2.3) the intermediate obtained from (1.2.2) is treated with a stream of nitrogen, and both a lithiumalkyl and a boronalkyl are used as (2).