The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 13, 1988

Filed:

Jan. 15, 1988
Applicant:
Inventors:

Akihiko Uchikawa, Yokkaichi, JP;

Koji Nishida, Yokkaichi, JP;

Yasuji Hosono, Yokkaichi, JP;

Kazuhisa Tachi, Yokkaichi, JP;

Takesi Okamoto, Yokkaichi, JP;

Yosuke Takai, Kako, JP;

Hideo Nakashima, Kako, JP;

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D04H / ;
U.S. Cl.
CPC ...
428219 ; 428288 ; 428296 ;
Abstract

There is provided a thermally bonded nonwoven fabric with a unit weight of 10 to 40 g/m.sup.2, comprising 20 to 100% by weight of a composite fiber with a fineness of 0.5 to 8 denier and 80 to 0% by weight of other fibers as the constituent fibers, the composite fiber comprising a first component which is an ethylene-.alpha.-olefin copolymer composition comprising an ethylen-.alpha.-olefin copolymer containing 0.5 to 4% by weight of an .alpha.-olefin having 4 to 12 carbon atoms blended with 0.01 to 0.3% by weight of a phenol type antioxidant and 0.01 to 0.3% by weight of a sulfur type antioxidant, having a Q-value (weight average molecular weight/number average molecular weight) of 4 or less, a density of 0.930 to 0.950 g/cm.sup.3, a melt flow rate of 5 to 50 g/10 min. and an oxidation induction time at 210.degree. C. of 10 min. or longer, and a second component which is a thermoplastic resin having a melting point higher by at least 20.degree. C. than that of the first component, with a constitutional ratio (sectional area ratio) of the first component to the second component being 35:65 to 70:30, said first component of the composite fiber forming at least a proportion of the fiber surface continuously along the length of each fiber and adhering through melting mutually the constituent fibers.


Find Patent Forward Citations

Loading…