The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 01, 1987

Filed:

Oct. 15, 1984
Applicant:
Inventors:

Morton M Wong, Placentia, CA (US);

Arnold L Shugarman, Santa Ana, CA (US);

Assignees:

Union Oil Co. of California, Los Angeles, CA (US);

Mono Power Co., Rosemead, CA (US);

Southern Pacific Land Co., San Francisco, CA (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C01B / ;
U.S. Cl.
CPC ...
423335 ; 423 38 ; 423 46 ; 423 98 ; 423109 ; 423150 ; 423D / ; 423340 ; 7510 / ; 75114 ; 75117 ; 75120 ; 75121 ;
Abstract

A process is provided for reducing the total concentration of heavy metals, notably lead, copper and zinc, naturally occurring in silica-rich sludge precipitated from geothermal brine in a brine handling system such as a geothermal brine electric generating plant. The process includes washing the sludge with hot water to displace any brine entrapped in the sludge, dewatering the washed sludge and leaching the silicious solids residue with hydrochloric acid having a concentration of between about 2 and about 9 weight percent and an acid-to-sludge weight ratio between about 0.10 and about 0.33. The acid-sludge mixture is heated to a temperature of at least about 50.degree. and the leaching time is at least about one hour. The leaching solution is separated from the leached sludge and the solids residue are washed with water. Preferably the water used in both washing steps is condensate of steam derived from the geothermal brine. Effluent from the process is preferably combined with the brine for reinjection.