The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 25, 1986

Filed:

Jul. 26, 1983
Applicant:
Inventors:

Terukatsu Miyauchi, Yokohama, JP;

Yoneichi Ikeda, Kamakura, JP;

Takao Nakagawa, Ichikawa, JP;

Toshio Tsutsui, Ichikawa, JP;

Tatsuji Kikuchi, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29B / ;
U.S. Cl.
CPC ...
264 12 ; 44 / ; 201-6 ; 201-8 ; 201 42 ; 264 14 ; 264 15 ; 264 296 ; 264 297 ; 264118 ; 264121 ; 264330 ;
Abstract

A two-step process for producing microspherical pitch or green coke particles having an average diameter of 30-200 .mu.m from finely divided petroleum or coal pitch having a softening point of 60.degree.-220.degree. C. and a fixed carbon content of 40-75 wt %. In the first step the material pitch is fluidized in the stream of a gas substantially inert to the pitch at a temperature of 100.degree.-800.degree. C., the mixed stream is rapidly cooled to 30.degree.-400.degree. C., and microspherical pitch particles are recovered with or without separate recovery of an oily product. In the second step the pitch spheres are further subjected to thermal cracking and polycondensation by use of a fluidized bed at a temperature of 350.degree.-520.degree. C. for a retention time of 1 min. to 3 hours, and microspherical green coke particles and a light cracked oil are recovered. In both steps a pressure between the ordinary level and 10 kg/cm.sup.2 is used.