The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jun. 04, 1985
Filed:
Feb. 28, 1983
Karl Seibert, Dueren-Niederau, DE;
Klaus Neumann, Kreuzau-Obermaubach, DE;
Ernst Spiess, Erftstadt-Gymnich, DE;
Hendrik G Bruil, Ede, NL;
Akzona Incorporated, Asheville, NC (US);
Abstract
A thickening agent comprising polyether derivatives of the general formula: ##STR1## wherein R.sub.1 is a substituted or unsubstituted hydrocarbon radical or an alkylphenol radical having 10 or more carbon atoms, n is 10 to 100, m is 0 to 25, and p is 1 to 3, and wherein R.sub.2 is an alkyl radical having 8 to 30 carbon atoms. These polyether derivatives are prepared by the gradual addition of a long-chain 1,2-epoxy having a chain length of 10 to 32 carbon atoms at temperatures from 100.degree. to 200.degree. C., to either (1) a polyethylene glycol monoether having an average molecular weight of 800 to 5000, the monoether group thereof being a substituted or unsubstituted hydrocarbon radical having at least 10 carbon atoms; or to (2) a polyethylene glycol-polypropylene glycol monoether with an average molecular weight of 850 to 6300, and having repeating ethylene oxide and propylene oxide units each forming a polyethylene glycol and polypropylene glycol block, respectively, the polypropylene glycol block having an average molecular weight of no more than 1300, and the monoether group forming the end of the polyethylene glycol block and being a substituted or unsubstituted hydrocarbon radical having at least 10 carbon atoms. This thickening agent is prepared using 0.1 to 1.0% by weight of an alkali hydroxide, referring to the total quantity of the long-chain epoxy and the monoether.