The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jan. 15, 1980
Filed:
Aug. 18, 1978
Edward N Balko, Trenton, MI (US);
Shyam D Argade, Woodhaven, MI (US);
James E Shrewsburg, Southgate, MI (US);
BASF Wyandotte Corporation, Wyandotte, MI (US);
Abstract
Fibers about micron size in cross-section of certain fluorine-containing polymers can be treated after being deposited as a diaphragm, either during operation or separately before installation, so that they develop a 0.25-millimeter-thick ply on either side of a central body which is substantially different in chemical composition. This yields a diaphragm 1 to 5 millimeters thick which has a Mullen burst strength approximately three to five times greater than that of an untreated diaphragm (20-25 pounds per square inch versus 5 to 7 pounds per square inch) and a remarkably improved service life in the treated diaphragm (200 days and up) in comparison with such untreated diaphragm (30 days or less). Use of a polymer based upon a major proportion of chlorotrifluoroethylene appears to be required. This discovery is economically significant, in that it is an essential element in the technology of the replacement of asbestos diaphragms now used with a synthetic material. Health-hazard and pollution-control considerations have made it desirable to replace asbestos, and this invention provides the key to the solution of the problem. Moreover, a synthetic-polymer diaphragm has two significant advantages that an asbestos one lacks--it will withstand washing or cleaning with an acid solution, and it does not swell in service and resists erosion, so that a closer electrode spacing can be used and the cell voltage can thus be lower.