The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 24, 1976

Filed:

Dec. 18, 1974
Applicant:
Inventor:

Armand E Brachman, Allentown, PA (US);

Assignee:

Bethlehem Steel Corporation, Bethlehem, PA (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B29D / ; B29F / ;
U.S. Cl.
CPC ...
264 455 ; 260 / ; 260 / ; 264 53 ; 264328 ; 264D / ; 264D / ; 264D / ; 428320 ;
Abstract

A process for producing a swirl-free, indent-free foamed thermoplastic structural article in which water is utilized as a foaming agent. Water and a melted thermoplastic resin are mixed together in an extruder to form a pressurized foamable mixture. The foamable mixture from the extruder is collected in an accumulator and from there is delivered to a cavity in a mold in a suitable clamping device. The pressure in the cavity is lower than the pressure of the foamable mixture in the accumulator or extruder therefore when the foamable mixture enters the cavity the foaming agent is released and the thermoplastic resin is frothed and expands to completely fill the cavity. The melted foamed thermoplastic resin cools in the mold and solidifies to form a foamed thermoplastic structural article. The quantity of water introduced into the extruder is between about 0.1 weight percent to about 0.5 weight percent of the thermoplastic resin charge in the extruder. To produce a swirl-free foamed thermoplastic structural article the quantity of water introduced into the extruder is between about 0.1 weight percent and about 2.0 weight percent of the thermoplastic resin charge in the extruder.