The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 06, 1976

Filed:

Dec. 04, 1974
Applicant:
Inventors:

Ryota Fujio, Akigawa, JA;

Nobuyuki Kataoka, Tokyo, JA;

Motozumi Kitayama, Tachikawa, JA;

Yoshihide Fukabori, Higashi-Murayama, JA;

Shiro Anzai, Higashi-Murayama, JA;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K / ; C08K / ; C08L / ;
U.S. Cl.
CPC ...
260 4221 ; 260 4233 ; 260 4242 ; 260 / ; 260 / ; 260 / ; 2608 / ;
Abstract

An ethylene-propylene copolymer rubber composition having a high Young's modulus, which comprises 100 parts by weight of a mixture of the following ingredients (a) and (b) in a weight ratio of ingredient (a)/ingredient (b) of 67/33-50/50, said ingredient (a) being an ethylene-propylene copolymer having a Mooney viscosity of at least 75, said ingredient (b) being divinylbenzene, (c) 0.3-2.5 parts by weight of an organic peroxide, and (d) 0.01-0.25 part by weight of sulfur, and the homogeneous rubber composition cured at 120.degree.-180.degree.C having a Young's modulus of 200-500 Kg/cm.sup.2, a tensile strength of at least 200 Kg/cm.sup.2, an elongation of at least 300%, a tear energy of at least 10 Kg/cm and retentions of Young's modulus and tensile strength at 70.degree.C of at least 50%.