The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 22, 2026

Filed:

Mar. 28, 2022
Applicants:

Arclin Usa Llc, Alpharetta, GA (US);

Harbisonwalker International Holdings, Inc., Moon Township, PA (US);

Inventors:

Shekhar L. Pendalwar, Lawrenceville, GA (US);

James T. Wright, Roswell, GA (US);

Lisa M. Arthur, Roswell, GA (US);

Darren A. Riedlinger, Roswell, GA (US);

Yusuf Celikbag, Roswell, GA (US);

Tomasz Ventz, Bethel Park, PA (US);

Assignees:

Arclin USA LLC, Alpharetta, GA (US);

Harbisonwalker International Holdings, Inc., Moon Township, PA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 61/06 (2006.01); B22D 41/02 (2006.01);
U.S. Cl.
CPC ...
C08L 61/06 (2013.01); B22D 41/02 (2013.01);
Abstract

A liquid phenolic resin composition for use as a binder for a refractory article, the phenolic resin composition comprising a phenol formaldehyde resin, wherein the phenolic resin composition has a reduced vaporization percentage of phenolic compounds. The phenolic resin composition is used in refractory compositions comprising at least 50 wt. % of one or more refractory aggregate(s), based on a total weight of the refractory composition. There is also disclosed a refractory article, such as a brick, formed into a shape comprising said refractory composition and heating until the phenolic resin composition is at least 20% cured and having a green strength after curing at 170° C. for 5 hours sufficient for handling the solid without falling apart. Ladles for transporting and pouring molten metals can be made with an inner liner formed by stacking at least two bricks along the bottom and sides of a ladle shaped metal outer liner, and then heating the stacked bricks to a temperature sufficient to carbonize the resin thereby forming the inner liner of the ladle.