The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 01, 2026

Filed:

Jun. 23, 2021
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Nobusato Morishige, Tokyo, JP;

Kazumi Mizukami, Tokyo, JP;

Ryutaro Yamagata, Tokyo, JP;

Takashi Kataoka, Tokyo, JP;

Haruhiko Atsumi, Tokyo, JP;

Daisuke Itabashi, Tokyo, JP;

Junichi Takaobushi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C21D 8/12 (2026.01); C21D 8/1216 (2026.01); C21D 8/1244 (2026.01); C21D 8/1277 (2026.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); H01F 1/147 (2006.01); H01F 41/00 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1255 (2013.01); C21D 8/1261 (2013.01); C21D 8/1272 (2013.01); C21D 8/1283 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/60 (2013.01); H01F 1/14775 (2013.01); H01F 41/00 (2013.01); C21D 2201/05 (2013.01); C22C 2202/02 (2013.01);
Abstract

A new and improved method for producing grain-oriented electrical steel sheet enabling production of grain-oriented electrical steel sheet realizing high magnetic flux density and excellent in magnetic characteristics, that is, as one aspect, a method for producing grain-oriented electrical steel sheet comprising a hot rolling process, cold rolling process, primary recrystallization annealing process, finish annealing process, and flattening annealing process, wherein shot blasting treatment and/or leveling treatment and treatment for contact with a solution are performed, the solution contains Cu etc. in a predetermined amount, the pH is −1.5 or more and less than 7, a solution temperature is 15° C. or more and 100° C. or less, and the time during which the steel sheet is dipped in the solution is 5 seconds or more and 200 seconds or less.