The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 04, 2026

Filed:

Jun. 30, 2023
Applicants:

Guangdong Brunp Recycling Technology Co., Ltd., Foshan, CN;

Hunan Brunp Recycling Technology Co., Ltd., Changsha, CN;

Hunan Brunp Ev Recycling Co., Ltd., Changsha, CN;

Inventors:

Shuaijun Xu, Foshan, CN;

Changdong Li, Foshan, CN;

Dingshan Ruan, Foshan, CN;

Weijian Liu, Foshan, CN;

Fengguang Li, Foshan, CN;

Weijia Zhang, Foshan, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); H01M 4/04 (2006.01); H01M 4/485 (2010.01); H01M 4/505 (2010.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); H01M 4/0471 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01);
Abstract

The invention discloses a mixing process for preparing a high nickel cathode material and its use. The mixing process is to add a precursor and a lithium source to a mixing device for mixing to obtain a mixture. After the mixture is uniformly mixed, the mixture is mixed. While the material equipment continues to operate, spray the liquid into the mixture. After the liquid spray is completed, the material is discharged, and the obtained mixture is put into a sagger for sintering. The liquid is pure water, ethanol, nitrogen methyl pyrrolidone, and additive solution. Or one or more of additive dispersions. The spray mixing process of the present invention can make the mixture more uniform, and because of the presence of a proper amount of mist droplets, the surface of the lithium source is slightly soluble in water and can adsorb the precursor.


Find Patent Forward Citations

Xu, Shuaijun. (2026). Mixing process for preparing high nickel cathode material and application thereof (U.S. Patent No. 12700590). U.S. Patent and Trademark Office. https://idiyas.com/patent/badge/12700590

Data source: USPTO (United States Patent and Trademark Office) public patent records. Weekly synchronization. How IDiyas builds this profile

Loading…