The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2026

Filed:

Apr. 08, 2021
Applicants:

Honda Motor Co., Ltd., Tokyo, JP;

Daido Steel Co., Ltd., Nagoya, JP;

Inventors:

Yoshiki Kumagai, Nagoya, JP;

Yoshinori Sumi, Nagoya, JP;

Shigeki Ueta, Nagoya, JP;

Hiroki Yamamoto, Tokyo, JP;

Isamu Saito, Tokyo, JP;

Assignee:

Daido Steel Co., Ltd., Nagoya, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/50 (2006.01); C21D 6/00 (2006.01); C21D 8/0221 (2026.01); C21D 8/0247 (2026.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/34 (2006.01); C22C 38/40 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/48 (2006.01); C22C 38/52 (2006.01); C22C 38/54 (2006.01); C22F 1/00 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0236 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 8/0226 (2013.01); C21D 8/0273 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/34 (2013.01); C22C 38/40 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/52 (2013.01); C22C 38/54 (2013.01); C22F 1/00 (2013.01);
Abstract

A seal member includes a γ' precipitation-hardening alloy, in which the γ′ precipitation-hardening alloy has a component composition of, in mass %: Ni: from 40 to 62%; Cr: from 13 to 20%; Ti: from 1.5 to 2.8%; Al: from 1.0 to 2.0% (provided that Ti/Al: 2.0 or less); Nb: 2.0% or less; Ta: 2.0% or less (provided that Nb+Ta: from 0.2 to 2.0%); B: from 0.001 to 0.010%; W: 3.0% or less; and Mo: 2.0% or less (provided that Mo+(½)W: from 1.0 to 2.5%), and optionally, C: 0.08% or less; Si: 1.0% or less; Mn: 1.0% or less; P: 0.02% or less; and S: 0.01% or less, with the balance being Fe and inevitable impurities, and in which the seal member has a hardness of 250 Hv or more, and includes a cold-rolled microstructure obtained by a cold rolling.