The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 30, 2026

Filed:

Oct. 25, 2021
Applicant:

Borealis Ag, Vienna, AT;

Inventors:

Qizheng Dou, Linz, AT;

Victor Sumerin, Kulloo, FI;

Elena Pomakhina, Linz, AT;

Jari Äärilä, Kulloo, FI;

Assignee:

BOREALIS GMBH, Vienna, AT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B29C 48/22 (2019.01); B29C 48/00 (2019.01); B29C 48/09 (2019.01); C08F 10/02 (2006.01); C08L 23/0807 (2025.01); B29K 23/00 (2006.01);
U.S. Cl.
CPC ...
C08L 23/0815 (2013.01); B29C 48/022 (2019.02); B29C 48/09 (2019.02); C08F 10/02 (2013.01); B29K 2023/08 (2013.01); C08L 2203/18 (2013.01); C08L 2205/025 (2013.01); C08L 2314/02 (2013.01);
Abstract

The invention relates to a polyethylene (PE) composition comprising a base resin which comprises (A) a first ethylene homo- or copolymer fraction, wherein fraction (A) has melt flow rate, MFR2, from 100 to 600 g/10 min; and (B) a second ethylene-1-hexene copolymer fraction, wherein fraction (A) has a lower molecular weight than fraction (B) and wherein fraction (B) is present in an amount of from 50.0 to 58.0 wt. % based on the total weight of the base resin; wherein the base resin has a content of units derived from 1-hexene from 0.44 to 0.79 mol % based on the total amount of base resin; wherein the base resin has a molecular weight distribution, being the ratio of Mw/Mn, from 32 to 40 and the base resin has a Z average molecular weight, Mz, of more than 1,500 kg/mol; wherein the polyethylene composition has a melt flow rate MFR5 from 0.10 to 0.25 g/10 min; and a melt flow rate ratio, FRR21/5, from 30 to 42; and wherein the polyethylene composition has a critical temperature, Tc, in the rapid crack propagation test of −10° C. or lower and not less than −25° C. The invention also relates to a PE composition obtainable by a multistage process, an article comprising a PE composition, a pipe and use of a PE composition comprising a base resin for producing an article.


Find Patent Forward Citations

Loading…