The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 30, 2026

Filed:

Jul. 07, 2021
Applicant:

Borealis Ag, Vienna, AT;

Inventors:

Andrey Buryak, Linz, AT;

Victor Sumerin, Kulloo, FI;

Franz Ruemer, Linz, AT;

Jari Aarila, Kulloo, FI;

Joy Jie Cheng, Linz, AT;

Assignee:

BOREALIS GMBH, Vienna, AT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 10/02 (2006.01); C08F 2/00 (2006.01); C08F 210/14 (2006.01); C08K 3/04 (2006.01); C08L 23/0807 (2025.01);
U.S. Cl.
CPC ...
C08F 10/02 (2013.01); C08F 2/001 (2013.01); C08F 210/14 (2013.01); C08K 3/04 (2013.01); C08L 23/0815 (2013.01); C08K 2201/019 (2013.01); C08L 2203/18 (2013.01); C08L 2314/02 (2013.01);
Abstract

The present invention relates to a polyethylene composition comprising a base resin which comprises (A) a first ethylene homo- or copolymer fraction, and (B) a second ethylene-hexene-1 copolymer fraction, wherein fraction (A) has a lower molecular weight than fraction (B) and wherein fraction (B) is present in an amount of from 51.0 to 58.5 wt. %, preferably 52.0 to 57.5 wt. %, more preferably 53.0 to 57.0 wt. % based on the total weight of the base resin, wherein fraction (B) of the base resin has a content of units derived from hexene-1 from 0.80 to 1.45 mol %, preferably of from 0.82 to 1.35 mol % and more preferably of from 0.85 to 1.30 mol %, wherein the base resin has a number average molecular weight Mn of 8,500 g/mol or higher, and wherein the polyethylene composition has a melt flow rate MFRs from 0.10 to 0.30 g/10 min, preferably from 0.15 to 0.28, and still more preferably from 0.16 to 0.25 g/10 min, to a process for producing the polyethylene composition, to an article, especially a pipe comprising the polyethylene composition and to the use of the polyethylene composition for the production of an article, especially a pipe.


Find Patent Forward Citations

Loading…