The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 23, 2026

Filed:

Mar. 17, 2021
Applicant:

Semiconductor Energy Laboratory Co., Ltd., Atsugi, JP;

Inventors:

Kazuhei Narita, Tokyo, JP;

Yohei Momma, Isehara, JP;

Shunpei Yamazaki, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/36 (2006.01); C01G 51/42 (2025.01); C01G 53/50 (2025.01); H01M 4/485 (2010.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/366 (2013.01); C01G 51/42 (2013.01); C01G 53/50 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01);
Abstract

A method for manufacturing a positive electrode active material with high charge and discharge capacity is provided. Alternatively, a method for manufacturing a positive electrode active material with high charge and discharge voltage is provided. Alternatively, a method for manufacturing a power storage device with little deterioration is provided. Alternatively, a method for manufacturing a highly safe power storage device is provided. Alternatively, a method for manufacturing a novel power storage device is provided. A method for manufacturing a secondary battery including a positive electrode active material is provided. A method for manufacturing the positive electrode active material includes a first step of synthesizing a first lithium source and a first transition metal source to form a first composite oxide; a second step of synthesizing an impurity source to provide an impurity layer for the first composite oxide after the first step; and a third step of synthesizing a second lithium source and a second transition metal source to form a second composite oxide after the second step and providing the second composite oxide over the first composite oxide provided with the impurity layer.