The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 23, 2026

Filed:

Jun. 06, 2023
Applicants:

Kansai Paint Co., Ltd., Amagasaki, JP;

Nissan Motor Co., Ltd., Yokohama, JP;

Inventors:

Shingo Sato, Kanuma, JP;

Mutsumi Yamazaki, Hiratsuka, JP;

Yuko Iwara, Yokohama, JP;

Tatsuya Suzuki, Yokohama, JP;

Hironori Tsutsui, Yokohama, JP;

Assignees:

KANSAI PAINT CO., LTD., Amagasaki, JP;

NISSAN MOTOR CO., LTD., Yokohama, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 5/06 (2006.01); B05D 3/06 (2006.01); B05D 7/00 (2006.01);
U.S. Cl.
CPC ...
B05D 5/066 (2013.01); B05D 3/063 (2013.01); B05D 7/572 (2013.01); B05D 7/574 (2013.01); B05D 2210/00 (2013.01); B05D 2401/10 (2013.01); B05D 2401/20 (2013.01); B05D 2502/005 (2013.01); B05D 2520/00 (2013.01); B05D 2601/08 (2013.01); B05D 2601/10 (2013.01); B05D 2601/20 (2013.01); B05D 2601/22 (2013.01);
Abstract

A method for forming a multilayer film, including: a step (1) of applying an aqueous two-pack first colored coating material on an automobile outer panel to form an uncured first colored coating film; a step (2) of applying an aqueous one-pack white color coating material on the uncured first colored coating film to form an uncured white coating film; a step (3) of setting the uncured white coating film for 4 minutes or more such that a resultant coating film has a solid content of 50% by mass or more; a step (4) of applying an aqueous one-pack interference color coating material on the uncured white coating film having the solid content of 50% by mass or more to form an uncured interference color coating film; a step (5) of applying a solvent-based two-pack clear coating material on the uncured interference color coating film to form an uncured clear coating film; and a step (6) of heating the coating films formed in the steps (1) to (5) at a temperature of 75° C. or more and to 100° C. or less to simultaneously cure the coating films.


Find Patent Forward Citations