The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 02, 2026

Filed:

Jun. 16, 2020
Applicant:

Dowa Electronics Materials Co., Ltd., Tokyo, JP;

Inventor:

Masanori Fujii, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01B 1/22 (2006.01); B22F 1/00 (2022.01); B22F 1/052 (2022.01); B22F 1/107 (2022.01); B22F 9/04 (2006.01); C09D 11/033 (2014.01); C09D 11/037 (2014.01); C09D 11/14 (2006.01); C09D 11/52 (2014.01); H01B 13/00 (2006.01);
U.S. Cl.
CPC ...
H01B 1/22 (2013.01); B22F 1/00 (2013.01); B22F 1/052 (2022.01); B22F 1/107 (2022.01); B22F 9/04 (2013.01); C09D 11/033 (2013.01); C09D 11/037 (2013.01); C09D 11/14 (2013.01); C09D 11/52 (2013.01); H01B 13/00 (2013.01); B22F 2301/255 (2013.01); B22F 2304/10 (2013.01);
Abstract

There are provided a silver powder, which is able to form an electrically conductive film having a lower resistance value than that of conventional electrically conductive films when the silver powder is used as the material of an electrically conductive paste which is fired to form the electrically conductive film, and a method for producing the same. A first silver powder having one peak or more, at each of which a frequency is a local maximum value in a volume-based particle size distribution obtained by measuring the first silver powder in a dry process by means of a laser diffraction particle size analyzer, is mixed with a second silver powder having two peaks or more, at each of which a frequency is a local maximum value in a volume-based particle size distribution obtained by measuring the second silver powder in a dry process by means of a laser diffraction particle size analyzer, to produce a silver powder having three peaks or more, at each of which a frequency is a local maximum value in a volume-based particle size distribution obtained by measuring the silver powder in a dry process by means of a laser diffraction particle size analyzer, the silver powder having one peak, at which a frequency is a local maximum value in a volume-based particle size distribution obtained by measuring the silver powder in a wet process by means of a laser diffraction scattering particle size analyzer.


Find Patent Forward Citations