The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 19, 2026

Filed:

Dec. 21, 2020
Applicant:

Sanyo Electric Co., Ltd., Kadoma, JP;

Inventors:

Takamitsu Tashita, Tokushima, JP;

Fumikazu Mizukoshi, Osaka, JP;

Akihiro Katogi, Tokushima, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/36 (2006.01); H01M 4/02 (2006.01); H01M 4/133 (2010.01); H01M 4/134 (2010.01); H01M 4/48 (2010.01); H01M 4/587 (2010.01);
U.S. Cl.
CPC ...
H01M 4/366 (2013.01); H01M 4/133 (2013.01); H01M 4/134 (2013.01); H01M 4/364 (2013.01); H01M 4/483 (2013.01); H01M 4/587 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01);
Abstract

A negative electrode for nonaqueous electrolyte secondary batteries is provided with: a negative electrode current collector; a first negative electrode mix layer arranged on a surface of the negative electrode current collector; and a second negative electrode mix layer arranged on a surface of the first negative electrode mix layer. The first negative electrode mix layer contains a first carbon material having a true density of 2.1 g/cmto 2.3 g/cm, the second negative electrode mix layer contains a second carbon material having a true density of 1.5 g/cmto 2.0 g/cm, the inter-particle porosity of the second carbon material in the second negative electrode mix layer is larger than that of the first carbon material in the first negative electrode mix layer, and the ratio of the mass of the first negative electrode mix layer to that of the second negative electrode mix layer is 95:5 to 80:20.


Find Patent Forward Citations