The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 19, 2026

Filed:

Jan. 29, 2021
Applicant:

Proterial, Ltd., Tokyo, JP;

Inventors:

Kousuke Kuwabara, Tokyo, JP;

Shuho Koseki, Tokyo, JP;

Assignee:

Proterial, Ltd., Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 30/00 (2006.01); B22F 10/28 (2021.01); B33Y 10/00 (2015.01); B33Y 40/20 (2020.01); B33Y 70/00 (2020.01); B33Y 80/00 (2015.01); C22C 1/04 (2023.01); C22F 1/16 (2006.01); F04D 29/02 (2006.01); F04D 29/28 (2006.01);
U.S. Cl.
CPC ...
C22C 30/00 (2013.01); B22F 10/28 (2021.01); B33Y 80/00 (2014.12); C22C 1/04 (2013.01); C22F 1/16 (2013.01); F04D 29/023 (2013.01); F04D 29/284 (2013.01); B22F 2203/11 (2013.01); B22F 2301/15 (2013.01); B22F 2301/205 (2013.01); B22F 2301/35 (2013.01); B22F 2304/054 (2013.01); B22F 2998/10 (2013.01); B22F 2999/00 (2013.01); B33Y 10/00 (2014.12); B33Y 40/20 (2020.01); B33Y 70/00 (2014.12); F05D 2230/40 (2013.01); F05D 2300/17 (2013.01);
Abstract

A production method for an alloy member having mainly high hardness and high resistance to corrosion and produced by an additive manufacturing method, the alloy member, and a product using the alloy member are provided. The production method of an alloy member includes: an additive manufacturing step of forming a shaped member through an additive manufacturing method using an alloy powder containing elements Co, Cr, Fe, Ni, and Ti each in a range of 5 atom % to 35 atom % and containing Mo in a range exceeding 0 atom % and 8 atom % or less, the remainder being unavoidable impurities; and a heat treatment step of holding the shaped member in a temperature range higher than 500° C. and lower than 900° C. directly after the additive manufacturing step without undergoing a step of holding the shaped member in a temperature range of 1080° C. to 1180° C.