The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 28, 2026

Filed:

Apr. 14, 2021
Applicant:

Salzgitter Flachstahl Gmbh, Salzgitter, DE;

Inventors:

Ingwer Denks, Wolfenbüttel, DE;

Jan Roik, Wolfenbüttel, DE;

Konstantin Molodov, Braunschweig, DE;

Assignee:

Salzgitter Flachstahl GmbH, Salzgitter, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/02 (2006.01); C21D 1/19 (2006.01); C21D 1/25 (2006.01); C21D 1/26 (2006.01); C21D 1/28 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C21D 8/0221 (2026.01); C21D 8/0247 (2026.01); C21D 9/48 (2006.01); C21D 9/52 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/20 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 9/52 (2013.01); C21D 1/19 (2013.01); C21D 1/25 (2013.01); C21D 1/26 (2013.01); C21D 1/28 (2013.01); C21D 6/005 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0273 (2013.01); C21D 9/48 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/20 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); C22C 38/38 (2013.01); C21D 2211/001 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

A method for producing a steel strip with a multiphase structure by which the production of complex geometries with a high energy-absorption capacity and high resistance to edge cracking is provided achieving a high yield strength or high yield-strength ratio and a high elongation at break, comprising producing a rolled steel strip of particular elements, and first annealing the steel strip at a temperature of between 750° C. and 950° C., and subsequently first cooling of the steel strip to a temperature of between 200° C. and 500° C. at an average cooling rate of 2 K/s to 150 K/s, further cooling of the steel strip to a supercooling temperature below 100° C. at an average cooling rate of 1 K/s to 50 K/s, final annealing of the steel strip with a Hollomon-Jaffe parameter, and final cooling of the steel strip to room temperature at an average cooling rate of 1 K/s to 160 K/s.