The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2026

Filed:

Dec. 24, 2021
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Takuya Mitsunobu, Tokyo, JP;

Hiroshi Takebayashi, Tokyo, JP;

Takehiro Takahashi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/01 (2006.01); B23K 11/11 (2006.01); B62D 27/02 (2006.01); F16B 5/08 (2006.01); B62D 29/00 (2006.01);
U.S. Cl.
CPC ...
F16B 5/08 (2013.01); B23K 11/11 (2013.01); B62D 27/02 (2013.01); B62D 29/00 (2013.01);
Abstract

The present disclosure inhibits liquid metal embrittlement (LME) cracking and improves corrosion resistance in a welded joint obtained by spot welding a first steel sheet and a second steel sheet. In the welded joint of the present disclosure, a first plating layer is provided on a surface of the first steel sheet facing the second steel sheet, no plating layer is present on or a second plating layer is provided on a surface of the second steel sheet facing the first steel sheet, a boundary plating layer is provided between the first steel sheet and the second steel sheet in a range of 0.5 mm from an end part of the corona bond of the spot welded part toward an outside of the spot welded part, and a Zn penetrated part is present at least at one of the first steel sheet and the second steel sheet adjoining the boundary plating layer. The Zn penetrated part advances from the boundary plating layer along the steel grain boundary, an Mg concentration at a front end of the Zn penetrated part at a location where a Zn concentration is 0.1 mass % is 0.20 mass % or less, and the first plating layer and the second plating layer satisfy a predetermined Relation I.