The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2026

Filed:

Mar. 31, 2022
Applicant:

Bmg Incorporated, Kyoto, JP;

Inventors:

Yoshifumi Okamoto, Tsukuba-city, JP;

Sujin Hoshi, Tsukuba-city, JP;

Fumiki Okamoto, Tokyo, JP;

Mikki Arai, Fukuoka-city, JP;

Shuhei Tanida, Kizugawa-city, JP;

Yusuke Kojitani, Kyoto-city, JP;

Motoki Fujimura, Kyoto-city, JP;

Woogi Hyon, Kyoto-city, JP;

Suong-Hyu Hyon, Uji-city, JP;

Assignee:

BMG Incorporated, Kyoto, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
A61L 24/10 (2006.01); A61L 24/00 (2006.01); A61L 24/08 (2006.01);
U.S. Cl.
CPC ...
A61L 24/108 (2013.01); A61L 24/0036 (2013.01); A61L 24/08 (2013.01); A61L 2430/16 (2013.01);
Abstract

In specific embodiments, provided is a material for preventing adhesion of membranes in an ophthalmic surgery for treatment of glaucoma or the like without using mitomycin-C or the like. Particularly provided is such material, which is easy to handle and has no risk of histolysis or infections. In a production method of a preferred embodiment, prepared are: aldehyde-modified dextran (first reactant) having weight-average molecular weight of 10,000-5,000,000 and introduced aldehyde group-per-anhydrous glucose unit (mol/AGU) of 0.4-0.7; and succinic anhydride-added poly-L-lysine (second reactant) having weight-average molecular weight of 1000-100,000 and having residual amino group ratio of 80-99%; then, they are mixed together so that aldehyde group-to-amino group molar ratio becomes 0.9-1.1 and are reacted in presence of water so that polymer concentration becomes 8-20%; and a hydrogel produced by the reaction, or a suspension before gelation, is freeze-dried to produce a porous sheet having a thickness of 0.1-0.8 mm.