The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 14, 2026

Filed:

Sep. 21, 2021
Applicant:

Vehicle Energy Japan Inc., Hitachinaka, JP;

Inventors:

Takeshi Miki, Hitachinaka, JP;

Shuichi Suzuki, Hitachinaka, JP;

Yusuke Tachikawa, Hitachinaka, JP;

Assignee:

Vehicle Energy Japan Inc., Hitachinaka, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/36 (2006.01); H01M 4/131 (2010.01); H01M 4/133 (2010.01); H01M 4/48 (2010.01); H01M 4/587 (2010.01); H01M 10/0525 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/364 (2013.01); H01M 4/131 (2013.01); H01M 4/133 (2013.01); H01M 4/48 (2013.01); H01M 4/587 (2013.01); H01M 10/0525 (2013.01); H01M 2004/027 (2013.01);
Abstract

A lithium ion secondary battery is provided which has a sufficient discharge capacity and has a low internal resistance in a low SOC range. The lithium ion secondary battery includes: a positive electrode including a positive electrode mixture containing a positive electrode active material represented by the following formula: LiMO; (where X satisfies −0.15≤X≤0.15, Mrepresents a group of elements including at least one selected from the group consisting of Mn and Al, Ni, and Co.); and a negative electrode including a negative electrode mixture containing a negative electrode active material containing a carbon-based material, a negative electrode additive containing a copper oxide, and a binder, in which the negative electrode mixture contains the copper oxide in an amount of 0.5 wt % or more and 15 wt % or less based on the total weight of the negative electrode active material and the negative electrode additive.