The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 31, 2026

Filed:

Mar. 17, 2021
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Hiroshi Hasegawa, Tokyo, JP;

Hideyuki Kimura, Tokyo, JP;

Noriaki Moriyasu, Tokyo, JP;

Sota Goto, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); B21C 47/02 (2006.01); C21D 8/0221 (2026.01); C21D 8/0247 (2026.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0226 (2013.01); B21C 47/02 (2013.01); C21D 8/0263 (2013.01); C21D 9/46 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C21D 2211/001 (2013.01); C21D 2211/008 (2013.01);
Abstract

After low-temperature finish rolling has been performed on a steel material having a certain chemical composition, cooling is performed at an average cooling rate of 10° C./s or higher to a temperature of 500° C., rapid cooling is further performed in a temperature range from a Ms temperature to a temperature of (Ms temperature-200° C.), coiling is thereafter performed in a low temperature range of 250° C. or lower, and the coiled steel sheet is uncoiled and further subjected to rolling with a certain amount or more of rolling load per unit width and the like. Consequently, it is possible to obtain a high-strength hot-rolled steel sheet having a microstructure including, in terms of area fraction, 95% or more of a martensite phase at a position located at ¼ of the thickness of the steel sheet, in which an average aspect ratio of prior austenite grains is 3.0 or more.