The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 17, 2026

Filed:

Mar. 25, 2020
Applicant:

Semiconductor Energy Laboratory Co., Ltd., Atsugi, JP;

Inventors:

Yohei Momma, Kanagawa, JP;

Mayumi Mikami, Kanagawa, JP;

Teruaki Ochiai, Kanagawa, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C01G 53/42 (2025.01); H01M 4/02 (2006.01); H01M 4/04 (2006.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
C01G 53/42 (2013.01); H01M 4/0471 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 10/0525 (2013.01); C01P 2002/72 (2013.01); C01P 2006/40 (2013.01); H01M 2004/028 (2013.01);
Abstract

A positive electrode active material with high capacity and excellent charge and discharge cycle performance, a positive electrode active material with high productivity, a positive electrode active material that suppresses a decrease in capacity, or the like is provided. Alternatively, a high-capacity secondary battery, a secondary battery with excellent charge and discharge characteristics, a highly safe or reliable secondary battery, or the like is provided. The positive electrode active material is obtained by a first heating step of heating a mixture of a first material, a second material, and a third material and a second heating step of heating a mixture which is a mixture of the mixture, a fourth material, and a fifth material and has a total amount of 15 g or more. The first material is a halogen compound including an alkali metal, the second material includes magnesium, the third material is a metal oxide including a metal A and cobalt, the fourth material includes nickel, and the fifth material includes aluminum. Each heating is performed in an atmosphere including oxygen. A temperature in the first heating step is lower than a temperature in the second heating step by 20° C. or more.