The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 03, 2026

Filed:

Oct. 20, 2017
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Quentin Bernardi, Paris, FR;

Tuan A. Mai, Richmond Hill, CA;

Nicolaas Van Der Borght, Herent, BE;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B23K 26/38 (2014.01); B23K 26/12 (2014.01); B23K 26/144 (2014.01); B23K 26/26 (2014.01); B23K 26/322 (2014.01); C21D 9/50 (2006.01); C23C 28/02 (2006.01); B23K 101/18 (2006.01); B23K 103/04 (2006.01);
U.S. Cl.
CPC ...
B23K 26/38 (2013.01); B23K 26/123 (2013.01); B23K 26/144 (2015.10); B23K 26/26 (2013.01); B23K 26/322 (2013.01); C21D 9/505 (2013.01); C23C 28/021 (2013.01); B23K 2101/185 (2018.08); B23K 2103/04 (2018.08); C21D 2211/001 (2013.01);
Abstract

A method for producing a precoated steel sheet () includes providing a precoated steel strip comprising a steel substrate carrying, on at least one of its faces, a precoating. The precoating includes an intermetallic alloy layer and a metallic alloy layer extending atop the intermetallic alloy layer. The metallic alloy layer is a layer of aluminum, a layer of aluminum alloy or a layer of aluminum-based alloy. The method also includes laser cutting the precoated steel strip so as to obtain at least one precoated steel sheet (). The precoated steel sheet () includes at least one cut edge surface (). The cut edge surface () includes a substrate region () and a precoating region () and the thickness of the precoated steel sheet () being comprised between 1 mm and 5 mm. The laser cutting is carried out such that it results directly in a reduced-aluminum zone (), extending over the entire height (h) of the cut edge surface () and over a length smaller than or equal to the length thereof. The surface fraction of aluminum on the substrate region () of the reduced-aluminum zone () directly results from the laser cutting operation being comprised between 0.3% and 6%.