The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 20, 2026

Filed:

Dec. 18, 2019
Applicant:

Voestalpine Stahl Gmbh, Linz, AT;

Inventors:

Wolfgang Ernst, Linz, AT;

Helmut Spindler, Oed-Öhling, AT;

Assignee:
Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 38/58 (2006.01); B23K 35/30 (2006.01); B23K 103/04 (2006.01); C21D 8/02 (2006.01); C21D 9/50 (2006.01); C21D 9/52 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/54 (2006.01);
U.S. Cl.
CPC ...
C22C 38/58 (2013.01); B23K 35/3073 (2013.01); C21D 8/0205 (2013.01); C21D 9/50 (2013.01); C21D 9/52 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01); B23K 2103/04 (2018.08);
Abstract

The invention relates to a method for producing thermomechanically produced hot strip products in which a steel alloy is melted; the steel alloy is adjusted so that a recrystallization during the hot rolling is suppressed; the final rolling temperature is greater than 800° C.; the melted steel alloy is cast into slab ingots and after being heated to a temperature above Ac, the slab ingots are hot rolled until they reach a desired degree of deformation and a desired strip thickness; after the rolling, the strip is cooled to room temperature and for hardening purposes, is briefly heated to a temperature >Ac3 and cooled again, characterized in that the heating takes place with a temperature increase of more than 5 K/s, more than 10 K/s, more than 50 K/s, or more than 100 K/s, and is kept at a desired target temperature for a period of 0.5 to 60 s before cooling to yield improved mechanical properties.