The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 20, 2026

Filed:

May. 12, 2022
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Masanori Takenaka, Tokyo, JP;

Minoru Takashima, Tokyo, JP;

Yukihiro Matsubara, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/12 (2006.01); C22C 38/00 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/34 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/60 (2006.01); H01F 1/10 (2006.01); H01F 1/16 (2006.01);
U.S. Cl.
CPC ...
C21D 8/1233 (2013.01); C21D 8/12 (2013.01); C21D 8/1222 (2013.01); C21D 8/1255 (2013.01); C21D 8/1272 (2013.01); C22C 38/00 (2013.01); C22C 38/008 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/34 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/60 (2013.01); H01F 1/16 (2013.01); Y02P 10/20 (2015.11);
Abstract

Provided is a method of producing a hot-rolled steel sheet for a grain-oriented electrical steel sheet. The method comprising: preparing a steel slab having a chemical composition containing, by mass %, C: 0.002% or more and 0.080% or less, Si: 2.00% or more and 8.00% or less, Mn: 0.02% or more and 0.50% or less, acid-soluble Al: 0.003% or more and less than 0.010%, and at least one of S or Se: 0.001% or more and 0.010% or less in total, with N limited to less than 0.006%, and the balance being Fe and inevitable impurities; heating the steel slab to 1300° C. or lower; and subjecting the steel slab to hot rolling, wherein a friction coefficient in final pass of the hot rolling is 0.35 or less.


Find Patent Forward Citations

Loading…