The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 13, 2026

Filed:

Jun. 26, 2023
Applicant:

Posco Co., Ltd, Pohang-si, KR;

Inventors:

Young-Roc Im, Gwangyang-si, KR;

Jong-Chan Park, Gwangyang-si, KR;

Jai-Hyun Kwak, Gwangyang-si, KR;

Min-Seo Koo, Gwangyang-si, KR;

Assignee:

POSCO CO., LTD, Pohang-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); B32B 15/01 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/54 (2006.01); C22C 38/58 (2006.01); C23C 2/02 (2006.01); C23C 2/06 (2006.01); C23C 2/28 (2006.01); C23C 2/40 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/013 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/02 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0247 (2013.01); C21D 8/0263 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01); C22C 38/58 (2013.01); C23C 2/02 (2013.01); C23C 2/0224 (2022.08); C23C 2/06 (2013.01); C23C 2/28 (2013.01); C23C 2/29 (2022.08); C23C 2/40 (2013.01); C21D 2211/001 (2013.01); C21D 2211/002 (2013.01); C21D 2211/003 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

Provided is a method of manufacturing a high-strength cold rolled steel sheet. The method includes: preparing a slab; heating the slab to 1,150° C. to 1,250° C.; finish hot rolling the heated slab within 900° C. to 980° C.; cooling the slab at an average cooling rate of 10° C./sec to 100° C./sec; winding the slab in 500° C. to 700° C.; cold rolling the slab at a cold-rolling reduction ratio of 30% to 60% to obtain a cold rolled steel sheet; continuously annealing the cold rolled steel sheet at Ae3+30° C. to Ae3+80° C.; primarily cooling the continuously annealed steel sheet at an average cooling rate of 10° C./s or less to 560° C. to 700° C. and secondarily cooling the steel sheet at an average cooling rate of 10° C./s or more to 270° C. to 330° C.; and reheating the cooled steel sheet at a temperature increase rate of 5° C./s or lower to a temperature in a range of 380° C. to 460° C.