The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 06, 2026

Filed:

May. 19, 2021
Applicant:

Global Graphene Group, Inc., Dayton, OH (US);

Inventor:

Bor Z. Jang, Centerville, OH (US);

Assignee:

Honeycomb Battery Company, Dayton, OH (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/00 (2006.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01); H01M 4/58 (2010.01); H01M 4/62 (2006.01); H01M 10/0525 (2010.01); H01M 10/0569 (2010.01); H01M 50/403 (2021.01); H01M 50/44 (2021.01); H01M 50/451 (2021.01);
U.S. Cl.
CPC ...
H01M 50/451 (2021.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 4/5825 (2013.01); H01M 4/622 (2013.01); H01M 10/0525 (2013.01); H01M 10/0569 (2013.01); H01M 50/403 (2021.01); H01M 50/44 (2021.01); H01M 2300/0037 (2013.01);
Abstract

A flame-resistant polymer composite separator for use in a lithium battery, wherein the polymer composite separator comprises (a) a binder or matrix polymer; (b) 0.1% to 50% by weight of a lithium salt dispersed in the polymer; and (c) from 30% to 99% by weight of particles or fibers of an inorganic material or polymer fibers that are dispersed in or bonded by the polymer, wherein the polymer is a polymerization or crosslinking product of a reactive additive comprising (i) a first liquid solvent that is polymerizable, (ii) an initiator or crosslinking agent, and (iii) the lithium salt and wherein the polymer composite separator has a thickness from 50 nm to 100 μm and a lithium ion conductivity from 10S/cm to 5×10S/cm at room temperature.