The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 30, 2025

Filed:

Dec. 15, 2020
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Dorien De Knijf, Denderhoutem Oost-Vlaanderen, BE;

Lode Duprez, Gentbrugge, BE;

Koenraad Theuwissen, Berchem, BE;

Tom Waterschoot, Lokeren, BE;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/60 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0226 (2013.01); C21D 8/0263 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/60 (2013.01); C21D 2211/001 (2013.01); C21D 2211/008 (2013.01);
Abstract

A hot rolled steel sheet having a composition including the following elements, 0.18%≤Carbon≤0.3%, 1.8%≤Manganese≤4.5%. 0.8%≤Silicon≤2%, 0 001%≤Aluminum≤0.2%, 0.1%≤Molybdenum≤1%, 0.001%≤Titanium≤0.2%, 0.0001%≤Boron≤0.01%, 0%≤Phosphorus≤0.09%, 0%≤Sulfur≤0.09%, 0%≤Nitrogen≤0.09%, 0%≤Chromium≤0.5%, 0%≤Niobium≤0.1%, 0%≤Vanadium≤0.5%, 0%≤Nickel≤1%, 0%≤Copper≤1%, 0%≤Calcium≤0.005%, 0%≤Magnesium≤0.0010% the remainder composition being composed of iron and unavoidable impurities caused by processing, the microstructure of said steel sheet including in area fraction, of at least 70% martensite, 8% to 25% residual austenite, wherein the shape factor of the residual austenite is between 4 and 12.