The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 23, 2025

Filed:

Jul. 04, 2019
Applicant:

Voestalpine Stahl Gmbh, Linz, AT;

Inventors:

Daniel Krizan, Linz, AT;

Katharina Steindeder, Linz, AT;

Reinhold Schneider, Wels, AT;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/38 (2006.01); C21D 1/26 (2006.01); C21D 9/52 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C21D 9/46 (2006.01);
U.S. Cl.
CPC ...
C22C 38/38 (2013.01); C21D 1/26 (2013.01); C21D 9/52 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C21D 9/46 (2013.01); C21D 2211/001 (2013.01); C21D 2211/003 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

A medium manganese cold-rolled steel intermediate product having an improved fts value is disclosed, the alloy having a carbon fraction within the range 0.003 wt %<C<0.12 wt %, a manganese fraction (Mn) within the range 3.5 wt %<Mn<12 wt %, a silicon fraction (Si) and/or an aluminium fraction (Al) as alloy fractions, where Si wt %+Al wt %<1, optionally further alloy fractions, optional microalloy fractions, in particular a titanium fraction (Ti) and/or a niobium fraction (Nb) and/or vanadium fraction (V), and the remainder of the alloy has iron (Fe) and unavoidable impurities of a melt. A method is also disclosed having the following step that is carried out after the cold-rolling step performing an intercritical box annealing process at a maximum annealing temperature of 684° C.−(517° C.*the carbon fraction in wt %).