The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 09, 2025

Filed:

Sep. 18, 2020
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Kazutoshi Takeda, Tokyo, JP;

Shuichi Yamazaki, Tokyo, JP;

Takuya Matsumoto, Tokyo, JP;

Hiroyasu Fujii, Tokyo, JP;

Masaru Takahashi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23C 22/20 (2006.01); C21D 9/46 (2006.01); C23C 22/82 (2006.01);
U.S. Cl.
CPC ...
C23C 22/20 (2013.01); C21D 9/46 (2013.01); C23C 22/82 (2013.01);
Abstract

There is provided a non-oriented electrical steel sheet that includes a base metal steel sheet and an insulating coating film that is formed on a surface of the base metal steel sheet, wherein the insulating coating film mainly contains metal phosphate, organic resin, and water-soluble organic compound, the water-soluble organic compound has an SP value that is within a range of 10.0 to 20.0 (cal/cm), the metal phosphate contains aluminum and zinc as metallic elements, and when measurement by an X-ray photoelectron spectroscopy is performed from a surface of the insulating coating film in a thickness direction of the non-oriented electrical steel sheet, a depth at which a strength of a 2p peak of zinc reaches a maximum is present closer to the surface side than a depth at which a strength of a 2p peak of aluminum reaches a maximum, and a maximum value of the strength of the 2p peak of zinc is 1 to 20 times a strength of the 2p peak of aluminum at the depth at which the strength of the 2p peak of zinc reaches a maximum.