The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 09, 2025

Filed:

Nov. 05, 2021
Applicant:

Lotte Chemical Corporation, Seoul, KR;

Inventors:

Sun Young Jung, Daejeon, KR;

Chang Kyu Son, Daejeon, KR;

Min Suk Jung, Daejeon, KR;

Hee Won Cho, Daejeon, KR;

Kyung Hoon Kim, Daejeon, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01D 67/00 (2006.01); B01D 71/26 (2006.01); C08L 23/06 (2006.01); C08L 23/12 (2006.01);
U.S. Cl.
CPC ...
B01D 67/0027 (2013.01); B01D 71/261 (2022.08); B01D 71/262 (2022.08); C08L 23/06 (2013.01); C08L 23/12 (2013.01); B01D 2323/081 (2022.08); B01D 2325/04 (2013.01); B01D 2325/24 (2013.01); B01D 2325/26 (2013.01); C08L 2205/025 (2013.01); C08L 2207/062 (2013.01);
Abstract

Disclosed are a polyolefin resin composition usable in manufacturing a single-layered dry porous membrane having excellent meltdown and shutdown properties, and a porous membrane using the polyolefin resin composition. The present invention provides a polyolefin resin composition for a porous membrane, wherein the polyolefin resin composition includes 30 wt % to 70 wt % of a high-density polyethylene having a melt flow index (190° C., 2.16 kg load) of 0.1 g/10 min to 5 g/10 min, a crystallization temperature of 115° C. to 125° C., and a degree of crystallinity of 75% or greater, and 30 wt % to 70 wt % of a high-crystallinity polypropylene having a melt flow index (230° C., 2.16 kg load) of 5 g/10 min to 20 g/10 min.