The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 02, 2025

Filed:

Oct. 12, 2018
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Yuya Kawai, Tokyo, JP;

Junichi Kitagawa, Tokyo, JP;

Yasuhide Oshima, Tokyo, JP;

Katsumi Kojima, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 1/02 (2006.01); B32B 15/09 (2006.01); B32B 15/18 (2006.01); B32B 27/08 (2006.01); B32B 27/20 (2006.01); B32B 27/36 (2006.01); B32B 37/18 (2006.01); B32B 38/00 (2006.01); B65D 65/40 (2006.01); B32B 1/08 (2006.01);
U.S. Cl.
CPC ...
B65D 65/40 (2013.01); B32B 15/09 (2013.01); B32B 15/18 (2013.01); B32B 27/08 (2013.01); B32B 27/20 (2013.01); B32B 27/36 (2013.01); B32B 37/182 (2013.01); B32B 38/0012 (2013.01); B32B 2038/0028 (2013.01); B32B 2264/102 (2013.01); B32B 2307/518 (2013.01); B32B 2439/00 (2013.01);
Abstract

A resin-coated metal sheet for a container includes: a metal sheet; a first resin coating layer provided on an inner face of the metal sheet after forming; and a second resin coating layer provided on an outer face of the metal sheet after forming, wherein a polar component of surface free energy of the second resin coating layer is 3.5 mN/m or more, after the second resin coating layer is subjected to heat treatment at a melting point of the second resin coating layer plus 8° C. for 2 minutes, and a static friction coefficient of the second resin coating layer, at 145° C., is 0.16 or less.