The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 07, 2025

Filed:

Jan. 13, 2023
Applicant:

Cpc Corporation, Taiwan, Kaohsiung, TW;

Inventors:

Yan-Shi Chen, Chiayi, TW;

Guo-Hsu Lu, Chiayi, TW;

Chi-Chang Hu, Chiayi, TW;

Chih-Yu Ku, Chiayi, TW;

Tien-Yu Yi, Chiayi, TW;

Assignee:

CPC CORPORATION, TAIWAN, Kaohsiung, TW;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01G 11/86 (2013.01); H01G 11/06 (2013.01); H01G 11/32 (2013.01); H01G 11/50 (2013.01); C25D 5/54 (2006.01);
U.S. Cl.
CPC ...
H01G 11/86 (2013.01); H01G 11/06 (2013.01); H01G 11/32 (2013.01); H01G 11/50 (2013.01); C25D 5/54 (2013.01);
Abstract

A method for prelithiating a soft carbon negative electrode includes the steps of: disposing the soft carbon negative electrode and a lithium metal piece spaced apart from each other with a lithium-containing electrolyte present therebetween; prelithiating the soft carbon negative electrode at a first constant C-rate until a voltage thereof is reduced to a first predetermined voltage not greater than 0.3 V vs. Li/Li, the first constant C-rate being not greater than 5 C; prelithiating the soft carbon negative electrode at a second constant C-rate until the voltage thereof is reduced to a second predetermined voltage lower than the first predetermined voltage, the second constant C-rate being not greater than 0.2 C and being less than the first constant C-rate; and prelithiating the soft carbon negative electrode at a prelithiation constant voltage which is not greater than the second predetermined voltage, thereby completing prelithiation of the soft carbon negative electrode.


Find Patent Forward Citations

Loading…