The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 07, 2025

Filed:

Apr. 15, 2021
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Keiichi Kondo, Tokyo, JP;

Yuji Arai, Tokyo, JP;

Keiichi Nakamura, Tokyo, JP;

Taro Oe, Tokyo, JP;

Takenori Kuramoto, Tokyo, JP;

Yosuke Takeda, Tokyo, JP;

Hiroki Kamitani, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/54 (2006.01); C21D 9/08 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01);
U.S. Cl.
CPC ...
C22C 38/54 (2013.01); C21D 9/08 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C21D 2211/001 (2013.01);
Abstract

The steel material according to the present disclosure consists of, in mass %, C: 0.15 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.05 to less than 0.80%, P: 0.030% or less, S: 0.0100% or less, Al: 0.100% or less, Cr: 0.30 to 1.50%, Mo: 0.25 to 2.00%, Ti: 0.001 to 0.015%, N: 0.0100% or less, O: 0.0050% or less, V: 0 to 0.05%, Nb: 0 to 0.010%, B: 0 to less than 0.0005%, Ca: 0 to 0.0100%, Mg: 0 to 0.0100%, and rare earth metal: 0 to 0.0100%, with the balance being Fe and impurities. In the steel material, the grain size number of prior-austenite grains is less than 7.0, Formula (1) to Formula (4) described in the specification are satisfied, the yield strength is 896 MPa or more, and the absorbed energy at −10° C. is 95 J or more.