The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 30, 2025

Filed:

Nov. 17, 2020
Applicant:

Lg Energy Solution, Ltd., Seoul, KR;

Inventors:

Hee-Won Choi, Daejeon, KR;

Tae-Gyun Noh, Daejeon, KR;

Mi-Ru Jo, Daejeon, KR;

Chan-Ki Park, Daejeon, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/1393 (2010.01); H01M 4/04 (2006.01); H01M 4/133 (2010.01); H01M 4/525 (2010.01); H01M 4/587 (2010.01); H01M 50/105 (2021.01); H01M 4/02 (2006.01); H01M 4/62 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/1393 (2013.01); H01M 4/0404 (2013.01); H01M 4/0435 (2013.01); H01M 4/133 (2013.01); H01M 4/525 (2013.01); H01M 4/587 (2013.01); H01M 50/105 (2021.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01); H01M 4/622 (2013.01); H01M 4/624 (2013.01); H01M 10/0525 (2013.01);
Abstract

A method for manufacturing a negative electrode, including the steps of preparing a negative electrode slurry including low-expansion natural graphite, a binder polymer, a conductive material and a dispersion medium; applying the negative electrode slurry to at least one surface of a negative electrode current collector, drying the coated negative electrode slurry, to form a preliminary negative electrode having a preliminary negative electrode active material layer; and pressing the preliminary negative electrode to obtain the negative electrode having a finished negative electrode active material layer. A difference between the specific surface area of the preliminary negative electrode active material layer before pressing and that of the finished negative electrode active material layer after pressing is 0.5 m/g to 1.0 m/g. A negative electrode obtained by the method and a secondary battery including the negative electrode are also disclosed.