The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 23, 2025

Filed:

Aug. 23, 2023
Applicant:

Heraeus Deutschland Gmbh & Co. KG, Hanau, DE;

Inventor:

Matthias Wegner, Hanau, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23C 8/12 (2006.01); C22C 1/02 (2006.01); C22C 5/04 (2006.01); C30B 35/00 (2006.01);
U.S. Cl.
CPC ...
C23C 8/12 (2013.01); C22C 1/02 (2013.01); C22C 5/04 (2013.01); C30B 35/002 (2013.01);
Abstract

Methods of making dispersion-hardened platinum compositions include A) producing a melt having at least 70 wt. % platinum, up to 29.95 wt. % of one or more of rhodium, gold, iridium and palladium, between 0.05 wt. % and 1 wt. % of oxidizable non-precious metals in the form of zirconium, yttrium and scandium, and, as the remainder, platinum including impurities, wherein the ratio of zirconium to yttrium in the melt is in a range of from 5.9:1 to 4.3:1 and the ratio of zirconium to scandium in the melt is at least 17.5:1, B) hardening the melt to form a solid body, C) processing the solid body to form a volume body, and D) oxidizing the non-precious metals contained in the volume body by a heat treatment in an oxidizing medium over a time period of at least 48 hours at a temperature of at least 750° C.