The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 09, 2025

Filed:

Jul. 24, 2020
Applicant:

Basf SE, Ludwigshafen am Rhein, DE;

Inventors:

Wolfgang Rohde, Ludwigshafen, DE;

Birgit Gerke, Ludwigshafen, DE;

Kerstin Schierle-Arndt, Ludwigshafen, DE;

Torben Adermann, Ludwigshafen, DE;

Matthias Voges, Ludwigshafen, DE;

Regina Vogelsang, Ludwigshafen, DE;

Assignee:

BASF SE, Ludwigshafen am Rhein, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22B 3/12 (2006.01); C01D 15/08 (2006.01); C22B 7/00 (2006.01); C22B 26/12 (2006.01); H01M 10/54 (2006.01);
U.S. Cl.
CPC ...
C22B 3/12 (2013.01); C01D 15/08 (2013.01); C22B 7/008 (2013.01); C22B 26/12 (2013.01); H01M 10/54 (2013.01); C01P 2002/72 (2013.01); C01P 2006/80 (2013.01);
Abstract

A process for the recovery of lithium from waste lithium ion batteries or parts thereof is disclosed. The process comprising the steps of (a) providing a particulate material containing a transition metal compound and/or transition metal, wherein the transition metal is selected from the group consisting of Mn, Ni and Co, and wherein further at least a fraction of said Ni and/or Co, if present, are in an oxidation state lower than +2, and at least a fraction of said Mn, if present, is manganese(II)oxide; which particulate material further contains a lithium salt and a fluoride salt, and which particulate material optionally contains calcium provided that the element ratio calcium to fluorine is 1.7 or less or is zero; (b) treating the material provided in step (a) with a polar solvent and an alkaline earth hydroxide; and (c) separating the solids from the liquid, optionally followed by washing the solid residue with a polar solvent such as water provides good separation of lithium in high purity, and recovery of valuable transition metals.


Find Patent Forward Citations