The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 26, 2025

Filed:

May. 25, 2020
Applicant:

Salzgitter Flachstahl Gmbh, Salzgitter, DE;

Inventor:

Manuel Otto, Cremlingen, DE;

Assignee:

Salzgitter Flachstahl GmbH, Salzgitter, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 26/32 (2014.01); B23K 9/16 (2006.01); B23K 26/24 (2014.01); B23K 103/04 (2006.01); C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/28 (2006.01); C22C 38/32 (2006.01);
U.S. Cl.
CPC ...
B23K 26/32 (2013.01); B23K 9/16 (2013.01); B23K 26/24 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); B23K 2103/04 (2018.08); C21D 2211/002 (2013.01);
Abstract

A welded component having mechanical properties in a welding seam region comparable or better to those in the non-influenced base material via a method including producing a hot-rolled steel product made of a high-strength air-hardenable steel with a material thickness of at least 1.5 mm having a chemical composition by mass in one embodiment of: C: 0.03 to 0.4; Mn: 1.0 to 4.0; Si: 0.09 to 2.0; Al: 0.02 to 2.0; P<=0.1; S<=0.1; N: 0.001 to 0.5; Ti: 0.01 to 0.2; Cr: 0.05 to 2.0; B: 0.001 to 0.1; Mo: 0.01 to 1.0; V: 0.01 to 0.2; optionally: Ni: 0.02 to 1.0; Nb: 0.01 to 0.1; and residual iron including conventional steel-accompanying elements, subsequently air hardening the produced hot-rolled steel product, then deforming the hot-rolled steel product in the air-hardened state to form a component, and producing welding connections using a fusion welding process on the component.