The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 29, 2025

Filed:

Mar. 14, 2022
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Keitaro Matsuda, Tokyo, JP;

Takuya Mitsunobu, Tokyo, JP;

Masaaki Uranaka, Tokyo, JP;

Jun Maki, Tokyo, JP;

Hiroshi Takebayashi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23C 2/06 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/38 (2006.01); C23C 2/02 (2006.01); C23C 2/16 (2006.01); C23C 2/28 (2006.01);
U.S. Cl.
CPC ...
C23C 2/06 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0236 (2013.01); C21D 8/0252 (2013.01); C21D 8/0278 (2013.01); C21D 9/46 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/38 (2013.01); C23C 2/022 (2022.08); C23C 2/16 (2013.01); C23C 2/285 (2013.01);
Abstract

High strength plated steel sheet having high hydrogen embrittlement resistance, that is, alloyed hot dip galvannealed steel sheet including steel sheet containing C: 0.05 to 0.40%, Si: 0.2 to 3.0%, Mn: 0.1 to 5.0%, and sol. Al: 0.4 to 1.50% and a alloyed hot dip galvannealed layer deposited on at least one surface of the steel sheet to 10 to 100 g/mand containing Fe: 5.0 to 15.0% and Al: 0.01 to 1.0%, having an internal oxidation layer including grain boundary oxides in a surface layer of the steel sheet, when examining a cross-section of a surface layer of the steel sheet, a Ratio A of the length of the grain boundary oxides projected an interface of the steel sheet and the alloyed hot dip galvannealed layer to the length of interface is 50% or more and 100% or less, and a surface depleted layer with a steel composition not including the grain boundary oxides which satisfies, by mass %, Si≤0.6% and Al≥0.05% is included at a depth of ½ of the average depth of the internal oxidation layer.


Find Patent Forward Citations